Insait long ol 'integrated steel' plent bilong nau, 'pellet ore' i save stap olsem nambawan samting bilong wokim ain long 'blast furnace'. Dispela wok bilong 'pelletization' i save prosesim ol gutpela paura bilong ain i kamap olsem ol 'spherical pellet' we i gat bikpela strong, na dispela i stretim hevi we ol i no inap putim gutpela paura i go insait long 'furnace'. Wok prinsipol bilong en i bruk long foapela bikpela hap: 'balling', draim na hatim pastaim, kukim long bikpela hat, na mekim i kol i go insait long ol pinis prodak, na kamapim wanpela gutpela fisikel na kemikel senis proses.

I. Taim bilong pilai bal: Kamapim ol grinpela bal

The balling stage marks the beginning of the pelletization process. The core involves mixing fine iron concentrate powder (with particle size < 0.074mm accounting for >80%), ol 'binder' (olsem 'bentonite') na wara insait long wanpela 'disc' o 'drum pelletizer', we ol i save kamapim ol 'spherical green ball' long rot bilong 'mechanical rolling' na 'capillary forces'. Long sait bilong bodi, aninit long wok bilong ol 'rotational' na 'centrifugal' fos, ol 'concentrate particles' i save pas na groa long wanpela 'layer' bihain long 'layer' wantaim gutpela 'core' olsem namel, na kamapim ol grinpela bal wantaim diamita bilong 8-16mm. Long sait bilong kemikel, ol 'binder' na wara i save kamapim ol 'liquid bridges' namel long ol liklik hap, na dispela i save strongim strong bilong ol grinpela bal long inapim ol samting we ol i nidim long kisim na mekim wok long hat.

II. Taim bilong draim na hatim pastaim: 'Dehydration' na 'consolidation'

Ol grinpela bal i go insait long 'grate', we ol i save rausim fri wara long hap bilong draim long 200-400 digri long stopim pairap long bikpela hat, na bihain ol i pinisim wok bilong strongim pastaim long hap bilong hatim pastaim long 900-1000 digri. Long dispela taim, magnetait (Fe3O4) insait long ol grinpela bal i save kamap 'hematite' (Fe2O3), na 'binder' i save go insait long ol 'sintering' riaksen long kamapim ol namba wan kristal koneksen, na dispela i save mekim strong bilong ol grinpela bal i kamap gutpela moa na i save putim as bilong kukim bihain.

III. Hai-Tempereture Roasting Stage: Crystal Reconstruction and Strength Enhancement

Ol grinpela bal we ol i bin hatim pinis i save go insait long 'rotary kiln' o 'grate kiln' bilong kukim long 1200-1300 digri, we em i ki bilong kamapim ol samting bilong 'pellet ore'. Ol liklik hap bilong 'hematite' i save kamap gen na gro, na kamapim wanpela strongpela kristal straksa; ol pipia olsem SiO2 na CaO insait long 'concentrate' i kamapim liklik hap bilong 'liquid phase', we i pulapim ol spes bilong ol liklik hap na i kamapim wanpela strongpela 'skeleton' bihain long em i kol, na dispela i mekim 'pellet ore' i stap strong na i no hat tumas. Long wankain taim, em i mekim ol 'iron oxides' i kamap gutpela olgeta, na dispela i mekim 'gred' na 'reducibility' bilong 'pellet ore' i kamap gutpela moa.

IV. Koling Stej: Pefomens Stabilisesen

Ol 'pellet ore' we ol i kukim long bikpela hat (inap 1000-1100 digri) i go insait long 'annular cooler', we ol i save winim kol win long mekim em i kol i go inap 100-150 digri. Kwik kol i save pasim kristal long kamap bikpela, na i save holim strongpela straksa na strong bilong 'pellet ore' na i save abrusim bagarap long ol narapela ikwipmen. Ol pipia ges we i gat bikpela hat long 300-400 digri we i kamap long taim bilong kol em ol i ken yusim gen long 'grate' bilong draim na hatim ol grinpela bal, na dispela i mekim na eneji i ron gut na daunim eneji we ol i yusim.

Long rot bilong bosim gut tempereja, win na taim bilong wanwan step, wok bilong 'pelletization' i save senisim 'low-grade fine iron concentrate paura i kamap gutpela 'pellet ore'. Wantaim wankain sais bilong ol liklik hap na gutpela 'reducibility', em inap long helpim 'blast furnace smelting' na gutpela bilong 'molten iron', na dispela i mekim em i kamap wanpela bikpela samting insait long 'modern iron and steel' indastri.

 

 